Introduction: The persistent challenge of biofouling on submerged marine structures demands effective protective strategies. This study investigates the concentration‑dependent antifouling performance and sustained field durability of silver nanoparticle (AgNP)‑reinforced polydimethylsiloxane (PDMS) coatings, where the AgNPs were synthesized via a phycocyanin‑mediated green route and incorporated at varying loadings to identify the optimal formulation for marine applications.
Methods: Phycocyanin extracted from Spirulina platensis served as a natural reducing and capping agent for AgNP synthesis under controlled conditions. Nanoparticles were characterized by XRD, TEM, FESEM, EDS, and UV–Vis spectroscopy, then incorporated into PDMS at 0.1–2 wt%. Evaluation included antibacterial and antialgal assays, ecotoxicity tests, and a 90‑day field immersion trial in the Persian Gulf. Biofouling quantified from 30‑day photos via CPCe software and analyzed by one‑way ANOVA (Tukey's, p<0.05; n=3).
Results: AgNPs were obtained as uniformly dispersed spherical particles (20–50 nm) with confirmed crystallinity. PDMS/AgNP coatings showed enhanced hydrophobicity (contact angle: 104°–110°). AgNPs exhibited potent antibacterial activity (96.25% against E. coli, MIC: 125 µg/mL; 95.62% against P. stutzeri, MIC: 250 µg/mL; 93.54% against S. aureus, MIC: 250 µg/mL), algal growth suppression against Nannochloropsis oculata (97.55% at 5 mg/mL), and 72‑h LC₅₀ values of 174.89 mg/L (A. salina) and 20.57 mg/L (A. amphitrite). PDMS with 2 wt% AgNPs produced inhibition zones of 18.2 mm (E. coli), ~17 mm (P. stutzeri), and 14.1 mm (S. aureus). After 90 days, the 2 wt% coating limited biofouling to 26.67%, versus 100% for uncoated panels and 80% for pristine PDMS.
Conclusions: Phycocyanin‑mediated green synthesis produced AgNPs with strong antimicrobial, antialgal, and antifouling properties. PDMS/AgNP nanocomposites demonstrated concentration‑dependent sustained field performance, offering a promising candidate, though further studies on silver release, coating degradation, and environmental exposure are needed.